FREE SHIPPINGFree shipping on all orders over 100000 INR.

Nitric Acid 68%

0
No votes yet

Product Qty Per Unit: 
60.00
Product usage unit: 
Kg.Liq

Negotiate Price

Product Delivery Locations: 
Mumbai, JNPT, Nhava Seva, Pirpav Jetty, Ballard Pier, Mumbai Port Trust, Butcher Island, ONGC EMR Shed, MIdc, Pune, Maharastra
Category: 
Tank Cleaner-20
Generic Name: 
Stainless Steel Passivation grade NITRIC ACID
Pasivation Grade Improve the corrosion resistance of parts made from austenitic, ferritic and martensitic corrosion-resistant steels of the 200, 300 and 400 series and precipitation hardened corrosion-resistant steels.
Product Description: 

Extra pure NITRIC , removes iron residue & forms an oxide layer that boosts the corrosion resistance of the stainless steel intended to improve the corrosion resistance of parts made from austenitic, ferritic and martensitic corrosion-resistant steels of the 200, 300 and 400 series and precipitation hardened corrosion-resistant steels.
High carbon, high chromium martensitic 440C grades which are selected for high hardness and resistance may be exempt from passivation treatments at the discretion of the procuring activity.

PRECAUTION :
1> Loose iron particles or other foreign particles must be removed or they will appear as rust or stain spots. may become smeared over or imbedded into the surface of corrosion-resistant steel parts.
2> DO avoid chlorides that, in excess, can cause a harmful flash attack. When possible, use only a good grade of water containing less than about 50 parts per million (ppm) of chlorides. Tap water is usually adequate, and in some cases up In several hundred ppm chlorides can be tolerated.


Chlorides: are present in many cleaning agents. This entails risk of pitting corrosion of stainless steel. If a cleaner containing chlorine, chlorides, bleaches orhypochlorites is used it must be afterwards promptly and thoroughly cleaned off.

Product Application: 

Transparent, colourless or yellowish corrosive liquid. A strong oxidizing agent that will attack allmost all metals.

Hazard: Dangerous fire risk in contact with orgenic materials. Highly toxic by inhalation, corrosive to the skin and mucous membrance. Uses : Orgenc synthesis (dyes, drugs,explosives, cellulose nitrate, nitrate salts ), photoengraving, etching steel. 

 

Passivation Treatments

• Grades with at least 16% chromium (except free machining grade such as 303):

20-50% nitric acid, at room temperature to 40oC for 30-60 minutes.

• Grades with less than 16% chromium (except free machining grades such as 416):

20-50% nitric acid, at room temperature to 40oC for 60 minutes.

• Free machining grades such as 303, 416 and 430F:

20-50% nitric acid + 2-6% sodium dichromate, at room temperature to 50oC for 25 40 minutes
 

Pickling Treatments

• All stainless steels (except free machining grades):

8-11% sulphuric acid, at 65 to 80oC for 5-45 minutes.

• Grades with at least 16% chromium (except free machining grades):

15-25% nitric acid + 1-8% hydrofluoric acid, at 20 to 60oC for 5-30 minutes.

• Free machining grades and grades with less than 16% chromium such as 303, 410 and 416: 10-15% nitric acid + 0.5-1.5% hydrofluoric acid, at 20 to 60oC for 5-30 minutes.

Product Procedure: 
Product Note: 
Product Technical Specification: 

Product pack size: 
500 GRM / 1 / 5 / 20 / 60 Kg. Pasivation Grade Improve the corrosion resistance of parts made from austenitic, ferritic and martensitic corrosion-resistant steels of the 200, 300 and 400 series and precipitation hardened corrosion-resistant steels.
Product alias: 
<p> Passivation grade NITRIC ACID for SS Treat</p>

Nitric Acid supplier in Mumbai, Kolkata, Chennai, Gandhidham, Fujairah - Dubai

Nitric Acid 68% manufacturer supplier distributor in Mumbai, Kandla, Kolkata, Vizag, Chennai, India, Fujairah, Dubai UAE, Muscat Oman, Kenya Africa. Get the best quality of Nitric Acid 68% at a competitive price from us. We have ready stock of Nitric Acid 68% in India, UAE Gulf, Oman, Kenya Africa. Contact us for bulk as well as small orders.

PROBLEM CLEARING AGENT COMMENTS
Rust and other corrosion products. Embedded or adhering "free iron Very light rust stain can be removed by 10% nitric acid. More significant rust or embedded iron will require picking. See also previous sections on Passivating and Picking. Sand or glass-bead blasting is another option Wear PPE as appropriate. Afterwards rinse well with clean water. Mix in acid-proof container, and be very careful with the acid, (See Precautions for acid cleaners)
Routine cleaning of boat fittings. Frequent washing down with fresh water. Recommended after each time the boat is used in salt water.
Cooking pot boiled dry. Remove burnt food by soaking in hot water with detergent, baking soda or amonia. Afterwards clean and polish. with a mild abrasive if necessary. See comments re steel wool.
Dark oxide from welding or heat treatment. "Picking Paste" or picking solutions given on previous page. Must be careful rinsed, and use care in handling (see Precautions for acid cleaners).
Scratches on polished (satin or brushed) finish. Slight scratches - use impregnated nylon pads. Polish with polishing wheel dressed with iron-free abrasive for deeper scratches. Follow polish lines. Then clean with soap or detergent as for routine cleaning Do not use ordinary steel wool - iron particles can become embedded in stainless steel and cause further surface problems. Stainless steel and "Scotchbrite" scouring pads are satisfactory.
Remarks: 

Nitric Acid (68%) Safety Data Sheet

Chemical Identity

Chemical Name

Nitric Acid

Chemical Classification

Inorganic Acid

Formula

HNO3

CAS Number

7697-37-2

UN Number

2031

Shipping Name

Nitric Acid

Codes / Label

Corrosive, Oxidiser, Class 8

Hazardous waste ID No.

16

Hazchem Code

2 PE

 

 

Physical / Chemical Data

Boiling Point / Range

120 Deg. C

Melting / freezing Point

- 40 Deg. C

PhysicalState

Watery Liquid

Specific Gravity

1.40

Solubility in water

Soluble

PH

Acidic

Appearance

Colourless to Brown

Odour

Choking Odour

 

Fire / Explosion Hazard Data

Flammability

No

LEL / UEL

Not Pertinent

Flash Point

Not Pertinent

Autoignition Temperature

Not Pertinent

Explosion Sensitivity to Impact

Stable

Explosion Sensitivity to Static Electricity

Stable

Hazardous Combustion Products

May emit poisonous oxides of
Nitrogen and Acid fumes

Oxidiser

Yes

Corrosive Material

Yes

Combustible / Flammable / Explosive Material

No

 

Preventive Measures
Avoid contact with liquid or vapours. Provide air mask, rubber acid suit, hood, boots, gloves, safety goggles, face shield to the workmen. Water shower and eyewash basin should be provided near the workplace.

Spills
Dilute with water and neutralise with alkali.

 

  • MUMBAI PORT NHAVA SEVASupply can be done within 1 Hour for BPT-Nhava.
  • Mumbai JNPT Ship Chandler50% Discount on every Marine chemical purchase.
  • Largest Marine CHEM SupplierStock Turbha, KANDLA, Vizag, Kolkata, Chennai.
  • Email Price, MSDS, Tech supportmarinechemical @ gmail.com

Top Rated Products