Sodium Silicate Water Glass
Silica gel production
Builder or anti-soil-redeposition agent for detergent
Peroxide stabilizer in bleaching for textile and pulp
Solubilizer in ink, flux binder for welding rods
Deflocculant for ceramic
Buffer
Fireproofing paper catalysts
Water treatment
Concrete hardner and acid-proof
Petroleum processing by emulsion breaking and corrosion prevention
Timber treatment.
Oil Field use
Range of Products:
We manufacture large range of Sodium Silicate both in Neutral and Alkaline grade of the typical qualities.
We also manufacture Sodium Silicate as per the customer's requirements and specification.
Sodium Silicates | Concentration | Mole Ratio | Baume |
Alkaline Sil | 40 - 54 % | 2.1 to 2.6 | 45 - 57 |
Neutral Sil | 27 - 39 % | 3.0 to 3.5 |
30 - 41.5 |
TESTING PROCEDURE :::
ANLYSIS PROCEDEURE OF SODIUM SILICATE : Take 5gm of sodium dilute it to 250ml in SMF with dist. Water , take 50 ml of the diluted solution add 2-4 drops of methyl red indicator. Then titrate it against IN {approx.} HCL Light Pink is the end point. Take this reading as “A” ml. To this solution add 5 gm of sodium fluoride dissolve properly add 6-7 drops of methyl red indicator titrate against IN HCL appearance of slight pink colour is the end point . Take this reading as “B” ml
CALCULATION For Na2O
“A”ml x 3.1 x normality of HCl = C%
Wt. Of sample
For Sio2
“B”ml x 15.02 x normality of HCl
Wt. Of sample X 10
Ratio of sodium silicate
% of SiO2 i.e D%
% of Na2o C%
Viscosity- AS PER IS 3944 B4 CUP
DETERMINATION OF IRON (as per Fe)
- Botanic Potassium Thiocynate ;- dissolve 1.0gm of potassium thiocynate in10ml of water. Add sufficient n-butano to makeup to 100ml. Shake vigorously until the solution is clear.
- Dilute H2SO4 :- approx.10%
- Standard Iron solution : weight 0.702gm of Ferrus Ammonium sulfate. Dissolve in 10ml dilute H2SO4 then make up 1000ml with water. Transfer 10 ml of this solution in 100ml M.Flask and make up 100ml with water. 1ml of this solution is equivalent to 0.01mg of iron
PRCEDURE :
- Sample Reading: take about 5gm of the sample accurately weighted. Dissolve it in distilled water and make the solution exactly 100ml. Take 10 ml of this solution add 1ml concentrated Nitric acid. Boil the solution and cool. Then transfer it into a nessler cylinder and add 30mg of Ammonium Persulfate and 15 ml of Botanic Potassium Thiocynate solution. Shake for 30 sec and allow the liquid to separate.
-
Blank reading : take 10 ml distilled water. Add 1ml concentrated Nitric acid boil the solution and cool. Then transfer it into a nesseler cylinder and add 30 mg of Ammonium Persulfate and 15 ml of Botanic Potassium Thiocynate solution . Shake for 30 sec. And allow the liquid to separate. Then add Standard Iron Solution until the colour of Butanol Layers in Both Cylinder (Sample & Blank)
CALCULATION :
Iron as Fe (%w) = 0.001 V
W
Where,
V= Volume in ml of Standard Iron Solution to add in Blank Reading
W= Weight in gm of sample
Sodium Silicate Water Glass manufacturer supplier distributor in Mumbai, Kandla, Kolkata, Vizag, Chennai, India, Fujairah, Dubai UAE, Muscat Oman, Kenya Africa. Get the best quality of Sodium Silicate Water Glass at a competitive price from us. We have ready stock of Sodium Silicate Water Glass in India, UAE Gulf, Oman, Kenya Africa. Contact us for bulk as well as small orders.